Chao,
Electroless plating on SU-8 is pretty tricky becasue the surface is
exteremely smooth. You can roughen the surface using oxyen/Fluorine plasma
or some wet process like permanganate etching. Look for papers from Georgia
Tech (I am sure there are others too) for more specific details on
roughening process.

Regards,
Dev

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
University Wafer
Addison Engineering
Process Variations in Microsystems Manufacturing