sokwon Paik
2006-01-11
Thomas,

  Journal of Vaccum science Technol. B 1998 16 (6) 3543-3546 could be the good
source for your refrerence.

  Good luck,

  Sokwon

Thomas Kiefer  wrote:
  Hi,

does anyone know a good adhesion promoter for PMMA on gold?
I'm using 35k PMMA, spin-coated on a thin gold layer. I'd like to
avoid using other metals to improve the adhesion. It should also be
possible to remove the adhesion promoter later easily.
Thanks!

Thomas,
EPFL, Lausanne
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
University Wafer