SU-8 layer less than 1 um
2006-01-12
Prem Pal
2006-01-12
Peter Svasek
2006-01-13
walter
2006-01-12
Brubaker Chad
SU-8 layer less than 1 um
Peter Svasek
2006-01-12
Prem,
we achieved a layer thickness of 0.54 um with diluted SU-8.
We diluted SU-8-50 with GBL (gamma-butyro-lactone).
The ratio was 1:1 by volume, which is 1 : 0.93 by weight  (SU-8-50 : GBL).
After adding the solvent, the mixture was stirred for 1 day using a
magnetic stirrer.
With a spinner speed of 4000 rpm (for 40 seconds) we got 0.77 um layer
thickness,
with 7000 rpm we got 0.54 um.


Best regards
Peter Svasek

Prem Pal wrote:

>Dear Researchers
>Which SU-8 should I use for depositing a layer of thickness less than 1 um. If
any have done it, please give me the recipe for achieving this thickness by spin
coating.
>Thanks in advance
>
>Prem Pal
>Yonsei University Seoul
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review