Hi Andrea,

Maybe you can try phosphoric acid at 80 degrees C, if you don't have
aluminium layers.

regards,
ck

---
Instrumentation Lab.
Microelectronics
TU Delft.

----- Original Message -----
From: 
To: 
Sent: Thursday, January 12, 2006 8:46 PM
Subject: [mems-talk] silicon nitride etch


>I am interested in chemical etching of silicon nitride LPCVD deposited.
> Actually, I'm using BHF, but it has a slow etch rate (10A/min). Is there
> something faster?
> Thanks
> Andrea
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
University Wafer
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation