MEMSnet Home: MEMS-Talk: dyed resist help
dyed resist help
2006-01-17
Jing Xue
dyed resist help
Jing Xue
2006-01-17
Dear All,

I am looking for the posssiblities of dyed resist. Can anyone be so
kind to share the expereience on this? Any inofrmation, such as
properties of dyed resist patterning, the vendor of the dyed resist,
etc. are greatly appreciated!

PS: dyed PMMA is perfered, but any dyed resist is welcom.

thanks a lot!

Jing
reply