RE: Piezoresistance coefficients of polysilicon
2006-01-18
Behraad Bahreyni
RE: Piezoresistance coefficients of polysilicon
Behraad Bahreyni
2006-01-18
The reported gauge factor for p-type polysilicon piezoresistors is about
20-30 and for n-type piezoresistors is -20 to -25. Check these
references for further information:

V. A. Gridchin, V. M. Lubimsky, and M. P. Sarina, “Piezoresistive
properties of polysilicon films,” Sensors and Actuators A: Physical,
vol. 49, no. 1-2, pp. 67–72, June 1995.

P. J. French, “Polysilicon: a versatile material for microsystems,”
Sensors and Actuators A: Physical, vol. 99, no. 1-2, pp. 3–12, April 2002.

B. Bahreyni and C. Shafai, “Fabrication of piezoresistive sensors in
standard mems foundry processes,” in Proceedings of the 4th IEEE
Conference on Sensors, Irvine, USA, November 2005.

Good luck,
Behraad

> Subject:
> [mems-talk] Piezoresistance coefficients of polysilicon
> From:
> JOJI JOYKUTTY 
> Date:
> Tue, 17 Jan 2006 04:26:08 -0800 (PST)
> To:
> [email protected]
>
> Hello to all,
>   Can any one give me the values of piezoresistance coefficients of
polysilicon. Will it be the same as that of single crystal silicon??? I need the
values for some simulations. I would be very grateful if you can send me some
references which deal with the piezoresistive properties of polysilicon.
>   Waiting for a response.
>   Regards,
>   Joji
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.