A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Solderable metallization recipe on glass & ceramics
Solderable metallization recipe on glass & ceramics
2006-01-23
Jauniskis, Linas
2006-01-23
Peter Svasek
2006-01-23
sokwon Paik
2006-01-23
walter
optical profilometer
2006-01-23
[email protected]
2006-01-23
ssood
microscope lens
2006-01-24
li cai
2006-01-24
David Nemeth
Solderable metallization recipe on glass & ceramics
Peter Svasek
2006-01-23
Linas,
20 nm Ti or Cr + 600...1000 nm Cu or Ag is ok
regards
Peter

Jauniskis, Linas wrote:

>Could anyone suggest an evaporated metallization (metal layers &
>thickness) recipe on glass & ceramics (alumina) that one can solder to
>with SnPb 63/37 and SnAg 96.5/3.5 solders.
>Thanks!
>Linas.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing