A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Solderable metallization recipe on glass & ceramics
Solderable metallization recipe on glass & ceramics
2006-01-23
Jauniskis, Linas
2006-01-23
Peter Svasek
2006-01-23
sokwon Paik
2006-01-23
walter
optical profilometer
2006-01-23
[email protected]
2006-01-23
ssood
microscope lens
2006-01-24
li cai
2006-01-24
David Nemeth
Solderable metallization recipe on glass & ceramics
sokwon Paik
2006-01-23
Linas,

  gold is the best metal for the soldering and of course Cr or Ti should be
deposited before gold deposition. With my experience, gold thickness should be
thicker than 0.5 micro meter for the soldering. If it is too thin then it is
very hard to solder and very easy to peeled off when you do the soldering. For
the safe soldering, I recommend thicker than 1 micro meter deposition and I
perfer electroplating as it make strong bonding surface. Evaporator may not be
suitable for the soldering.....

  sokwon

"Jauniskis, Linas"  wrote:
  Could anyone suggest an evaporated metallization (metal layers &
thickness) recipe on glass & ceramics (alumina) that one can solder to
with SnPb 63/37 and SnAg 96.5/3.5 solders.
Thanks!
Linas.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Nano-Master, Inc.
MEMS Technology Review