Ni and Cr etching
Neal Ricks
2006-01-31
Have you tried ferric chloride [i.e. iron(III)
chloride ]?

--- biqin huang  wrote:

> Does anyone kow the etchants for Ni and Cr which
> doesn't attack Gold thin
> film?