HI,

I have a wafer with trenches that are 3 um deep and 20 um wide.  I
want to planarize the wafer using a CMOS compatible material while not
exceeding a temperature of 650C.

I presume I cannot use BPSG for this purpose since it reflows only at
950C.I could use Polyimide but I am not sure if it is CMOS compatible.

Can anyone please suggest an alternative that suits the above requirements.

Thanks
Kamesh
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Mentor Graphics Corporation
Addison Engineering