A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Encapsulant for wire bonding
Encapsulant for wire bonding
2006-02-09
FrançoisTherriault Proulx
2006-02-10
Jesse D Fowler
RE : [mems-talk] Encapsulant for wire bonding
2006-02-10
Sebastien Allard
2006-02-09
Sebastien Allard
Is chromium mask is chromium oxide or chromium?
2006-02-10
sokwon Paik
Is chromium mask chromium or chromium oxide or both?
2006-02-10
sokwon Paik
2006-02-10
[email protected]
Encapsulant for wire bonding
[email protected]
2006-02-10
We agree!

We use Nail Polish (Enamel, not regular) and we thin it with a little
acetone. Clear nail polish so you can inspect the bonds.

We have also used Scotchguard.  You have to spray it in a bottle to collect
enough.

Nail polish provides less bubbles and a much cleaner finish.

Margaret

From: Fran s Therriault Proulx
        

Hi,
I'm a new subscriber to this mems-talk group and I'm not sure that my message
has been sent the first time. Sorry if it's the second time you receive it.

I'm looking for a kind of encapsulant to use with wire bonding. It is for a
MEMS
application. It should cover entirely wires. It has to insulate wires
electrically, but also be quite hard to accept pressure like a gentle
pushing of a finger. The material after cure has to become as wide as high due
to wires specifications and alignment. It cannot cures at high
temperatures(maximum aroud 170 Celsius). I think that NoSweep from Polyscience
should match my needs but I'm not sure. Does anyone know other products that
could help me to solve my problem? Is NoSweep a good solution for my problem?

Thank you
Sincerely yours
Frank


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Tanner EDA by Mentor Graphics
MEMS Technology Review