A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: diffusion barrier for copper-polyimide
diffusion barrier for copper-polyimide
2006-02-10
erkin seker
2006-02-10
Michael D Martin
PVDF vendor
2006-02-10
Shivalik Bakshi
decrease total thickness variation
2006-02-11
Andrea Mazzolari
2006-02-12
shay kaplan
2006-02-13
gtomblin
2006-02-17
Bill Moffat
diffusion barrier for copper-polyimide
erkin seker
2006-02-10
Hi,

I am trying to make micro strain gauges using the following method in
summary:

- Spin 250nm-thick polyimide diluted with NMP; completely cure at 325C
- Sputter/pattern 80nm-thick Cu/Ni on cured polyimide
- Spin 250nm-thick polyimide diluted with NMP; completely cure at 325C

The problem I am having is that after the cure, the polyimide above Cu/Ni
layer is disappearing.  I read about copper oxide diffusion into polyimide
due to the reaction between copper and polyamic acid; but I am not sure if
this explains the material loss over the metal lines.

I already tried amino silane adhesion promoters provided by GE Silicone, but
didn't have any success.

I would be grateful if somebody could suggest a solution.

Thank you very much.

erkin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
The Branford Group
University Wafer