Undercut uniformity of Gold wet etching
2006-02-14
X.P. Zhu
2006-02-14
Ad Hall
Undercut uniformity of Gold wet etching
Ad Hall
2006-02-14
Mopa,

Try the following.

1)  HMDS treat the wafer before coat.
2)  Bake the wafer for 1hr at 100c before etch to improve the resist.
3)  A good KI/I2/H2O mix 2 grams/0.5 grams/75 ml

Ad

-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of X.P. Zhu
Sent: Tuesday, February 14, 2006 2:55 AM
To: [email protected]
Subject: [mems-talk] Undercut uniformity of Gold wet etching

Hi,
    I am using KI/I2 to etch gold pattern. The
thickness of the gold layer which is on 2 inch wafer
is more than 1.5 micron. The etching rate at the edge
of the wafer is faster and in center it is slower. So
when the pattern in center is OK the undercut at the
edge will be not accepted (often > 3 micron). How to
reduce the undercut? Thank you for any advice.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing