MEMSnet Home: MEMS-Talk: silicon nitride: mechanism leading to intrinsic stress
Thermal Etching Conditions for Yttria Stabilized Zirconia
2006-02-22
avinash balakrishnan
silicon nitride: mechanism leading to intrinsic stress
2006-02-24
Andrea Mazzolari
silicon nitride: mechanism leading to intrinsic stress
Andrea Mazzolari
2006-02-24
Silicon Nitride deposited by LPCVD result in a tensile stress ranging from
90-1000 MPa.
This tensile stress is the sum of a thermal stress (compressive) and an
intrinsic stress (tensile). The last one is very dependent on deposition
condition. Which is the mechanism which lead to intrinsic stress formation?

Many thanks
Andrea

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
University Wafer
Mentor Graphics Corporation