Drilling glass.
Craig Friedrich
2006-03-01
I use plated diamond drills from Amplex.


g.balsubra manian wrote:

>Hi everybody.,
>
>I am looking for drill bits for drilling glass. If
>anyone have idea of suppliers providing drill bits in
>the range of 500-700 micrometer (0.5mm-0.7 mm), pls
>Inform me.
>
>Thanks
>
>Cheers.,
>Bala.
>_______________________________________________
>Hosted by the MEMS and Nanotechnology Exchange, the country's leading
>provider of MEMS and Nanotechnology design and fabrication services.
>Visit us at http://www.mems-exchange.org
>
>Want to advertise to this community?  See http://www.memsnet.org
>
>To unsubscribe:
>http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>
>


--
Craig R. Friedrich, PhD, PE
Professor of Mechanical Engineering
Director, Multi-Scale Technologies Institute
Dept of Mechanical Engineering – Engineering Mechanics
815 RL Smith
Michigan Technological University
1400 Townsend Drive
Houghton, MI 49931

Office: MEEM 906
Phone:  906-487-1922
Fax:    906-487-2822

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
MEMS Technology Review
Mentor Graphics Corporation