MEMSnet Home: MEMS-Talk: Drilling glass.
Drilling glass.
2006-03-01
g.balsubra manian
2006-03-01
Craig Friedrich
2006-03-01
Gareth Jenkins
2006-03-01
Scott D Cambron
2006-03-01
[email protected]
Drilling glass.
Gareth Jenkins
2006-03-01
Hi

Look for diamond engraving bits - I get these from RS Components (in the
UK).
For smaller diameter bits I have sometimes used dental drill bits (or
burs). Have a look at Diama :
http://www.diamadental.co.uk/
I have only ever tried the spherical tipped burs but other shapes may
also work. You may have to contact them for the sizes - there is some
correlation with the code number but I can't recall what.

Gareth

g.balsubra manian wrote:

>Hi everybody.,
>
>I am looking for drill bits for drilling glass. If
>anyone have idea of suppliers providing drill bits in
>the range of 500-700 micrometer (0.5mm-0.7 mm), pls
>Inform me.
>
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics