MEMSnet Home: MEMS-Talk: Balco (Ni 70% + Fe 30%) wire bonding on Ni/Au pads.
Wire bonding problems
2006-02-27
Stanley R. Shanfield
2006-02-28
Kenneth Smith
2006-02-28
David Nemeth
Balco (Ni 70% + Fe 30%) wire bonding on Ni/Au pads.
2006-03-01
PRAMOD GUPTA
2006-03-02
Adamson, Steve
Balco (Ni 70% + Fe 30%) wire bonding on Ni/Au pads.
PRAMOD GUPTA
2006-03-01
Hi

  Do you have any idea whether Balco (Ni 70% + Fe 30%) wire of 0.002" dia can be
bonded on Ni/Au pads by using thermosonic/ultrasonic technique or not? If yes,
who can do it?

  With regards,

David Nemeth  wrote:
  One possible solution would be to use a very small dab of silver conductive
epoxy after bonding. Epotek makes such an epoxy, although it is also
available from a variety of other sources.


David Nemeth
Senior Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA 20151


-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Stanley R. Shanfield
Sent: Monday, February 27, 2006 2:50 PM
To: [email protected]; [email protected]
Subject: [mems-talk] Wire bonding problems


We are trying to manually wire bond to thin (~.2 micron) Pt/Au on glass.
Although we get good bonds on test wafers at the time the metal is
deposited, the bonding is very unreliable after it has gone through more
processing (i.e. at wire pull test, the wire falls off, leaving the pad
intact,& undamaged; or the pull strength is low). The wafer sees anodic
bonding conditions at one point in our process sequence, and the sawing
process can leave scratches on the pads (the scratches do not penetrate the
metal).

Going up in bonding energy, time and force is a concern, since the glass
sometimes forms fissures under the bonding area at more extreme bonding
conditions, and a subsequent wire pull creates a pull-out from the glass. It
does not seem to help anyway. These bonds have to survive a ~350C
temperature excursion, so a pull-out is a concern.

Has anyone ever dealt with a problem like this? Any advice or observations?
You input would be much appreciated!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
The Branford Group