Dear All,
I evaported Cr and Au to the InGaAs/InP material.And I etched Au with KI:I2:H2O
etachant then etched Cr with KMnO4.But there are a very thin Cr layer can't
etch.Can you help me?
Thanks!

Zhang Zhenfeng