A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Electroplating onto SU-8
Electroplating onto SU-8
2006-03-04
Iskandar Samad
2006-03-04
g.balsubra manian
2006-03-05
Pradeep Dixit
2006-03-05
g.balsubra manian
Electroplating onto SU-8
g.balsubra manian
2006-03-04
Sputtering may not work as the Su-8 couldnot be
exposed to higher temperatures.So you can go with
electroless plating of Cr/Ti .Thats better. Then go
for the electroplating.

Cr forms oxide too.So you have tp take steps to remove
CR oxide otherwise Cr oxide is bad conductor and
adhesion with Cu will be a prob.

Bala.

--- Iskandar Samad  wrote:

> Hi all, Im looking to electroplate some copper onto
> SU-8 photoresist and
> was wondering if anyone has had experience with
> this. Btw, the SU-8 has
> been prepatterned and cured on a silicon wafer.
>
> Are there any issues about whether the
> sputtered/evaporated seed layer
> (for plating) adheres well to the SU-8, and if so
> what material seed
> would you suggest? Is there any material I could pre
> deposit that could
> perhaps aid adhesion?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.