A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Thermal Growth silicon dioxide
Thermal Growth silicon dioxide
2006-03-08
Hui Han
2006-03-08
Shay Kaplan
2006-03-09
Martin J Prest
2006-03-09
Leo Petrossian
2006-03-10
Roger Brennan
Thermal Growth silicon dioxide
Martin J Prest
2006-03-09
For oxide growth rate, see this:

http://ee.byu.edu/cleanroom/OxideThickCalc.phtml

Select 'wet' for steam oxidation.

I'm not an expert in this, but I guess wafers should be loaded and removed in a
nitrogen atmosphere.

Regards,

Martin.

-------------------------
Dr. Martin Prest
Research Fellow
Emerging Device Technology Research Centre
The University of Birmingham
U.K.
-------------------------

> -----Original Message-----
> From: Hui Han [mailto:[email protected]]
> Sent: 08 March 2006 15:49
> To: [email protected]
> Subject: [mems-talk] Thermal Growth silicon dioxide
>
> Hi, all,
>    I need some help in thermal growth SiO2, including the
> detailed steps
> (for example, if the Si sbustrate are directly interted into
> and removed
> out from the tube furnance or not), the rough growth rate.
>
>    I want to use water steam to promote the oxidation.
>
> Thanks for helps.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.