MEMSnet Home: MEMS-Talk: can Ag be a adhesive layer between Au and Si?
can Ag be a adhesive layer between Au and Si?
2006-03-13
[email protected]
Platinized silicon
2006-03-13
Hui Han
can Ag be a adhesive layer between Au and Si?
[email protected]
2006-03-13
Hello All,

people usually use Ti or Cr as an adhesive layer between Au and Si,

as far as I know, Ag can stick on silicon too, why people do not use
silver as an adhesive layer?

best

Yu Chen