MEMSnet Home: MEMS-Talk: thin film metal deposition
transparency mask
2006-03-20
Rupesh Sawant
thin film metal deposition
2006-03-20
D. Zhou
2006-03-20
sokwon Paik
2006-03-21
[email protected]
2006-03-21
matt estes
2006-03-21
g.balsubra manian
thin film metal deposition
D. Zhou
2006-03-20
Dear all,

Could anyone please recommend some methods of thin-film (<15 nm) metal
deposition? The requirements include good control over the thickness, good
uniformity of the layer and an ability to monitor the sheet resistivity. (
Is thermal evaporation a good option?) Many thanks.


--
Da-xiang Zhou
PhD candidate
Semiconductor Physics Group
Cavendish Laboratory
University of Cambridge

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Addison Engineering
University Wafer