Steph,

General composition of over 99% of all positive resists.  1) about 10% solvents
alcohols. molecular weight up to 200. 2) About 40% sensitizer usually a diazo
quinone molecular weight up to 5,000.  When this is exposed to U.V. light it
breaks down to indene carbo-oxylic acid. About 50% polymers usually a
Formaldehyde with a moleculer weight up to 60 to 80 thousand. When the resist
ages the polymer grows to molecular weight over 100,000 and it settles out of
the resist into gel slugs.  When you expose the resist and wash it in a basic
solution Tetra Methyl Ammonium Hydroxide it preferentially eats the acididc
areas.  You develop the exposed areas.  Hope his helps. Bill Moffat Yield
Engineering Systems

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
University Wafer
Mentor Graphics Corporation