MEMSnet Home: MEMS-Talk: how to etch the sputtered Ni mask?
how to etch the sputtered Ni mask?
1998-07-10
ZOU Qiang
how to etch the sputtered Ni mask?
ZOU Qiang
1998-07-10
Dear  All :

Recently I used Ni as mask for Si RIE. I found that it is easy to etch Ni
formed by electroplating. However it is very difficult to etch Ni formed by
sputtering. Would you please tell me how I can photoetch sputtered Ni mask?

Thank you very much!

ZOU  Qiang


email: [email protected]