A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: AZ4562
Electroplating Equipment Set-up
2006-03-05
J.J wang
2006-03-05
g.balsubra manian
2006-03-20
J.J wang
2006-03-20
g.balsubra manian
AZ4562
2006-03-21
steph champ
2006-03-21
Shay Kaplan
2006-03-21
abdou sar
2006-03-22
steph champ
AZ4562
steph champ
2006-03-22
Thanks for your answers about AZ4562

I have another question, I currently use the S1818, and the photoactive
compound is diazonapthoquinone
with a A Novalac Resin as binder and the PGMEA as solvent.
Do you have an idea of the photoactive compound in AZ4562 (given the binder
and the solvent are the same) ? Is it the same as AZ4562 ?

Steph

>From: "Shay Kaplan" 
>Reply-To: General MEMS discussion 
>To: "'General MEMS discussion'" 
>Subject: RE: [mems-talk] AZ4562
>Date: Tue, 21 Mar 2006 17:15:11 +0200
>
>Steph
>This is a most regular novolak based resist. Very much the 1518 etc just
>with higher solid content and viscosity to give the thickness.
>Shay
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics