Hi all,

I recently started to try AZ4903 photoresist in order to coat thick PR
films. I found that it is much more viscous than other types such as
AZ1518, AZ4620, so I always had bubbles when dispensing the
photoresist directly by pouring it on wafers. Do you any suggestions
about the best way to dispense it? Our spinner does not have a spray
function so this method is not available...

Thanks,
PJ

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering
Harrick Plasma, Inc.