MEMSnet Home: MEMS-Talk: Boron Diffusion
Boron Diffusion
2006-03-30
Vinay
Boron Diffusion
Vinay
2006-03-30
Hello All,
We are looking for companies which do deep boron diffusion on Si
Wafer. We are looking for depths in the range of 15-25um and boron
concentration in excess of 10e19. The Si wafers are 2" in diameter and
200-250um thick. If any of you could forward to me some information in
this regard, it would be greatly appretiated.

Thanks,
vinay