MEMSnet Home: MEMS-Talk: Is there any way to etch a hole through on siliconwafer?
Is there any way to etch a hole through on silicon wafer?
2006-04-03
Jeff chen
Is there any way to etch a hole through on siliconwafer?
2006-04-03
Shile
Is there any way to etch a hole through on silicon wafer?
2006-04-03
Florian Herrault
Is there any way to etch a hole through on silicon wafer?
2006-04-07
Leo Petrossian
native silicon oxide growth rate
2006-04-09
li cai
2006-04-10
Duan
Is there any way to etch a hole through on silicon
2006-04-04
Carel Heerkens
Is there any way to etch a hole through on siliconwafer?
Shile
2006-04-03
You can etch through the wafer with a crystallographic etch, such as KOH
or TMAH, which will result in sidewalls with ~55 degree inclination on a
<100> wafer.  Or you can etch through the wafer with ~vertical sidewalls
using RIE, e.g. Bosch Etch.  The laser approach is probably
unnecessarily expensive.  The wafer is normally grounded during RIE.
Grounding also might help if you hit the wafer with lightening:)

Roger Shile

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of Jeff chen
Sent: Monday, April 03, 2006 1:17 PM
To: [email protected]
Subject: [mems-talk] Is there any way to etch a hole through on
siliconwafer?

Hi,

I am working on a project which needs to etch a hole through the
silicon wafer (525 micron thick). The hole diameter is around 50
micron.
Does anyone have experience to do that?
Is there any way to do that? Etching? Laser excimer? or grounding
technology?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.