2006-04-03
Jeff chen
Is there any way to etch a hole through on siliconwafer?
2006-04-03
Shile
Is there any way to etch a hole through on silicon wafer?
2006-04-03
Florian Herrault
Is there any way to etch a hole through on silicon wafer?
2006-04-07
Leo Petrossian
native silicon oxide growth rate
2006-04-09
li cai
2006-04-10
Duan
Is there any way to etch a hole through on silicon
2006-04-04
Carel Heerkens
Is there any way to etch a hole through on silicon wafer?
Florian Herrault
2006-04-03
Him

This is very easy to do using ICP etching if this hole is the first step of
your process. Aspect ratio might be achieved up to 1:20 but 1:10 is already a
reasonnable challenge.

Laser machining silicon does give smooth sidewalls as compared to ICP.

Florian


Quoting Jeff chen :

> Hi,
>
> I am working on a project which needs to etch a hole through the
> silicon wafer (525 micron thick). The hole diameter is around 50
> micron.
> Does anyone have experience to do that?
> Is there any way to do that? Etching? Laser excimer? or grounding
> technology?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMStaff Inc.