dip-coating superhydrophobic coating
Matthew Coda
2006-04-05
Properly applied (vapor or liquid deposited) silane or siloxane based
SAMs are very robust on native oxide-on-silicon and certainly should not
be damaged by exposure to water (including immersion for long periods).
It's a matter of using an appropriate deposition strategy.  Even better
it doesn't have to be particularly complicated, I've done this using a
three component solution and a simple dip deposition.

-Matt

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of yilei zhang
Sent: Wednesday, April 05, 2006 10:04 AM
To: [email protected]
Subject: [mems-talk] dip-coating superhydrophobic coating

Dear Colleagues,
Could anyone recommend a simple dip-coating solvent for superhydrophobic
coating? My sample is silicon and rough, so the spin-coating TEFLON may
not
work well, plus it looks very expensive. For silane SAM, it was reported
water may damage the coating, so anyone have any suggestions?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review