yilei zhang
2006-04-12
Glukh, Konstantin
Is dry N2 environment necessary for FDTS coating?
Glukh, Konstantin
2006-04-12
Dry environment is absolutely necessary. The key to making good SAMs is
in having hydrophilic sample surface but no water in solution. Otherwise
you will end up with a lot of FDTS conglomerates in solution that will
precipitate on your sample.
BR,
Konstantin


-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of yilei zhang
Sent: Tuesday, April 11, 2006 4:12 PM
To: [email protected]
Subject: [mems-talk] Is dry N2 environment necessary for FDTS coating?

Dear colleagues:
Could anyone confirm whether the dry N2 environment is necessary in
preparing FDTS mixture and during dip-in coating? I found different
procedures about the SAM coating. Thank you very much.

Regards,
Yilei Zhang
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMS Technology Review
Addison Engineering