MEMSnet Home: MEMS-Talk: Re: Is dry N2 environment necessary for FDTS coating?
Re: Is dry N2 environment necessary for FDTS coating?
2006-04-12
Marco Doms
2006-04-12
Matthew Coda
Re: Is dry N2 environment necessary for FDTS coating?
Marco Doms
2006-04-12
As FDTS reacts vigorously with water, a dry atmosphere is quite useful. I
have always used a normal laminar flow hood in a dry environment and tried
to act as quickly as possible.
Why do you want to do a dipping process? A vapor phase deposition is
faster, not more complicated and gives better results!
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
The Branford Group
Mentor Graphics Corporation
University Wafer