Metal Removal Process on PMMA
Jayna Shah
2006-04-19
Hi All,

I have a lift-off pattern made of 0.75 microns thick Au with a base layer of 5
nm Cr on poly(methyl methacrylate) (PMMA) substrate.  I am wondering if anyone
has a  lift-off etch process that I can adapt.   I am aware that Si lift-off
metallization does not work on plastics, and I have to use etch chemistry.

Also, does anyone have any experience with shadow masks for deposition of 0.75
microns thick metal for the smallest feature size of 50 microns?

Thanks,
Jayna
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.