A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Silicon Ramp Needed
Silicon Ramp Needed
2006-04-20
[email protected]
2006-04-20
Richard H. Morrison
2006-04-20
David Nemeth
2006-04-20
William Lanford-Crick
2006-04-20
[email protected]
2006-04-20
Bill Moffat
2006-04-20
Behraad Bahreyni
2006-04-20
Beggans Michael H IHMD
Silicon Ramp Needed
[email protected]
2006-04-20
Are you willing to grind the slope?  The 5 um width is a little scary but the
rest seems pretty straight forward.

Roger Brennan
Solecon Labs

-----Original Message-----
>From: "[email protected]" 
>Sent: Apr 19, 2006 6:44 PM
>To: [email protected]
>Subject: [mems-talk] Silicon Ramp Needed
>
>OK Mems people, work with me. This is a real question.  How can I make a
>silicon ramp 5um tall on one end and 1um on the other, 250um long, 5um
>wide?  I'm starting with a 5um layer of Si on a substrate.  The real
>question is how to etch/make a smooth, ramp, type structure.  I feel a few
>lith steps of 1um 4 times to build "stairs" and then figure a way to smooth
>the 1um steps.  Anyone????
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Mentor Graphics Corporation
MEMS Technology Review