A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Silicon Ramp Needed
Silicon Ramp Needed
2006-04-20
[email protected]
2006-04-20
Richard H. Morrison
2006-04-20
David Nemeth
2006-04-20
William Lanford-Crick
2006-04-20
[email protected]
2006-04-20
Bill Moffat
2006-04-20
Behraad Bahreyni
2006-04-20
Beggans Michael H IHMD
Silicon Ramp Needed
William Lanford-Crick
2006-04-20
        Sounds interesting--What about grayscale lithography and dry
etching?

        William Lanford-Crick
        Micro and Nanotechnology Laboratory and
        Department of Electrical and Computer Engineering
        University of Illinois at Urbana-Champaign


Subject: [mems-talk] Silicon Ramp Needed

        OK Mems people, work with me. This is a real question.  How can I
make a
        silicon ramp 5um tall on one end and 1um on the other, 250um long,
5um
        wide?  I'm starting with a 5um layer of Si on a substrate.  The real
        question is how to etch/make a smooth, ramp, type structure.  I feel
a few
        lith steps of 1um 4 times to build "stairs" and then figure a way to
smooth
        the 1um steps.  Anyone????
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review
University Wafer