Hi All,
We are trying to measure the depth of P diffusion in N-type Si, using
the Staining technique. I tried using the etchant HF-HNO3[100:1]
mixture, but the stain was not very evident. I do not know the reason
for this. I would appreatiate any comments on this.

Thanks,
vinay