A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: forming boron and arsenic doped sidewalls in a siliconwafer
forming boron and arsenic doped sidewalls in a silicon wafer
2006-05-04
[email protected]
forming boron and arsenic doped sidewalls in a siliconwafer
2006-05-05
Kirt Williams
forming boron and arsenic doped sidewalls in a siliconwafer
2006-05-06
Roger Brennan
forming boron and arsenic doped sidewalls in a silicon wafer
2006-05-06
[email protected]
forming boron and arsenic doped sidewalls in a siliconwafer
Roger Brennan
2006-05-06
If you are willing to make the trench first and then dope, Plasma Immersion
Ion Implant (PIII) has been touted as a good way to dope sidewalls.  Any
number of furnace doping methods should work -- including BN and other disks
used as a doping source.

Roger Brennan
Solecon Labs

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of
[email protected]
Sent: Thursday, May 04, 2006 4:24 PM
To: [email protected].
Subject: [mems-talk] forming boron and arsenic doped sidewalls in a
siliconwafer


I am trying to form boron and arsenic doped sidewalls in trenches in a
silicon wafer.  I thought of doing reactive ion or electrochemical etching
of the trench bottom after isotropic doping, but I'm worried that the
reaction will be hard to time correctly because the silicon underneath would
etch much faster than the doped layer.  Any thoughts you have on the most
efficient process to form doped sidewalls would be greatly appreciated.

Thanks,

Daniel
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Mentor Graphics Corporation