Hello everyone,

I am trying to do some electroless nickel plating using Technic Inc,
solutions. I am having a problem in patterning this nickel, I tried to use a
sacrificial photoresist but the electroless nickel plating is not very
selective its plating everywhere. Any suggestions on this?

Ravi