2006-05-09
Hi.,

Electroless plating is used for plating on substrates
including non-conductor.Thats is based on the reducing
agent (electrons) available from the plating solution.

Electroplationg was used for plating on substrates on
only conductors.here current provides electrons which
acts as reudicng agent. So electroplating is selective
than electroless plating.

Best Wishes.,

Bala.

--- Zhang Xiao Qiang  wrote:

> Why do not you try electroplating? It will e
> selective.
>
> Thank you & have a nice day!
> Best regards!
>
> XiaoQiang
>
> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]] On Behalf Of
> ravi deverkadra
> To: [email protected]
> Subject: [mems-talk] Electroless Nickel Plating
>
> Hello everyone,
>
> I am trying to do some electroless nickel plating
> using Technic Inc,
> solutions. I am having a problem in patterning this
> nickel, I tried to use a
> sacrificial photoresist but the electroless nickel
> plating is not very
> selective its plating everywhere. Any suggestions on
> this?
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review