MEMSnet Home: MEMS-Talk: Masking layer for pyrex etching
Masking layer for pyrex etching
2006-05-09
Terry Zhu
2006-05-09
David Nemeth
2006-05-10
Gareth Jenkins
2006-05-10
ravi deverkadra
2006-05-10
Glenn Silveira
Masking layer for pyrex etching
Terry Zhu
2006-05-09
Hi,

  Thanks, Ravi and Gareth. I guess the electroplating is needed for 15um
nickel. It is very thick layer.  Do you think sputtering a thin  layer of
gold/Cr good for masking layer or other capable thin films?

  Regards,

  Terry