MEMSnet Home: MEMS-Talk: Can PMMA work as mask for dry etching on II-VI(ZnSe based) semiconductors?
Can PMMA work as mask for dry etching on II-VI(ZnSe based) semiconductors?
2006-05-17
jiaxing Yang
Can PMMA work as mask for dry etching on II-VI(ZnSe based) semiconductors?
jiaxing Yang
2006-05-17
I tried RIE etching with Cl2, the PMMA was etched
away.
any one has experience in this kind of etching? which
kind of gas can etch ZnSe but not PMMA?
Thanks!!
reply