Dear All ,

      I am using PECVD silicon nitride as a structural layer and Aluminum as
a sacrificial layer. First i want the patterning of nitride layer by RI
etching then wet etching of Aluminum layer ( releaging step ).
So if any know then please tell me what is recipe to etch the nitride layer
and the selectively by using PPR as a mask. what etchant i can use for
releasing step which will not attack on nitride layer.



Regards,
Deepak
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
University Wafer
Nano-Master, Inc.