A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Problem in etching buried oxide
Problem in etching buried oxide
2006-05-02
Julie Verstraeten
2006-05-02
David Nemeth
2006-05-04
ZICKAR Michaƫl
2006-05-05
walter essinger
2006-05-02
Beggans Michael H IHMD
2006-05-18
Mandar Deshpande
2006-05-26
Micro Sense
2006-05-27
Micro Sense
Problem in etching buried oxide
Micro Sense
2006-05-26
Hi Julie,

I am also working on DRIE in SOI. I would like to remind you of the fact
that DRIE is a pretty expensive process and that SiO2 (Mask) / Si
selectivity is roughly about 1:100. So I would suggest that you first plasma
clean your trench on either side for prolonged time (I do it for about 30
min @ 980 W) to completely remove the passivating layer and then do a HF
vapour etch or even a buffered HF wet etch (after you have etched top and
bottom trenches). This should actually work. Do let me know how you solved
this issue.

Cheers,
Vijay
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group