RE>Looking for Polyimide suppliers
3/25/98 4:12 PM
We use EPY-500 for installation of Si strain gages. Our supplier is
BLH Electronics, Inc.
75 Shawmut Road, Canton, MA 02021
Tel. (617) 821-2000
Tatyana Ishutkina
--------------------------------------
Date: 3/24/98 5:48 PM
To: Tatyana Ishutkina
From: mems-cc
Hi;
Does anybody know about the ployimide which has good adhesion with Si and
those suppliers? In my case, adhesion is so important. Any
information would be welcome.
Thanks.
--------
RFC-822 Header:
RECEIVED: from DARKSTAR.ISI.EDU by [146.115.43.50] ; 24 MAR 98 17:47:53 UT
Received: (from daemon@localhost)
by darkstar.isi.edu (8.8.7/8.8.6) id OAA15008
for mems-out-list; Tue, 24 Mar 1998 14:35:04 -0800 (PST)
Received: (from mems@localhost)
by darkstar.isi.edu (8.8.7/8.8.6) id OAA15000;
Tue, 24 Mar 1998 14:35:03 -0800 (PST)
Message-Id: <[email protected]>
Date: Tue, 24 Mar 1998 11:21:57 -1000 (HST)
From: Cheol-Hyun Han
Subject: Looking for Polyimide suppliers
To: [email protected]
X-URL: http://mems.isi.edu/mems.html
Reply-To: Cheol-Hyun Han , [email protected]