A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Help with Processing AlGaAs Broad Area Lasers
Help with Processing AlGaAs Broad Area Lasers
2006-05-30
ahajjiah
2006-05-30
PRAMOD GUPTA
2006-05-30
Jobert Van Eisden
2006-05-30
[email protected]
Help with Processing AlGaAs Broad Area Lasers
[email protected]
2006-05-30
Hello Ali, when you mean etching to the substrate do you mean all the way
through the active region.  Normal BA lasers are isolated only by etching
the contact layer and perhaps some of the cladding.

Also, is it necessary for you to put metal first?  Its seems easier to use
photolithography to isolate, than pattern again and deposit the metal with a
lift-off.  There should be no reason to etch the metal on a BA laser.

If you need do a metal first process, can you use a different gold etch such
as iodine based?  Also, you could use 1:8:80 sulf:peroxide:water for etching
the AlGaAs. I don't have much experience with more durable resist-Im sure
someone will provide feedback on that.

Good luck,

Scott



-----Original Message-----
From: ahajjiah [mailto:[email protected]]
Sent: Tuesday, May 30, 2006 10:08 AM
To: General MEMS discussion; mems-talk
Subject: [mems-talk] Help with Processing AlGaAs Broad Area Lasers


Dear All,

I am currently trying to process Broad Area Lasers on 1cm2 AlGaAs sample. On

the Epi side i am depositing Ti/Au by e-beam evaporation. Then using
photolithography to create openings on the sample to isolate the devices
from
each other by etching all the way to the substrate using wet etching. The
photoresist i am using is a positive photoresist (S1813).

My problem is this:

I know that (3 HCl:1 HNO3) will etch Au and AlGaAs and HF will etch Ti, but
my
photoresist will not hold against either etchants. As a result, my
photoresist
will not cover and protect the areas i don't want to be etched.

Can someone please suggest a solution for my problem?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
MEMS Technology Review
Nano-Master, Inc.