Hi, dear all,

Now I have a large trench (1mm wide, 1mm long, 4 um deep)  in the si
substrate. I'd like to fill some material and make the surface flat.  The
whole sample is 1" by 1".

Could you give me some suggestions how to do it?

Many thanks!

yours,

Ying Cai


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation