Hi Nupur,

I'm about to start using BPR100 and am lead to believe that the temperature
of the developer is extremely important. The sales rep who supplied it
informed me that the temperature must be 40DegC (the developer turns a milky
colour at this temperature) or it would not work.

Hope this helps,

Novak