A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PDMS bonding.,
PDMS bonding.,
2006-06-10
g.balsubra manian
2006-06-12
Joseph Grogan
2006-06-13
Gareth Jenkins
2006-06-13
Joseph Grogan
2006-06-14
Gareth Jenkins
2006-06-14
Joseph Grogan
2006-06-13
Ali Bhagat
2006-06-15
Gareth Jenkins
2006-06-13
lumiaoÂÀÃç
2006-06-15
huy vo
PDMS bonding.,
Joseph Grogan
2006-06-12
I've found it to be a couple minutes (maybe 1-3 minutes).  It might even
be bonded in 30 seconds or so, but I never tried to pull it apart in
less than a minute. But if it's only been 10-20 seconds, you can
definitely pull it apart. However, I found that if you pull it apart
during those first few seconds and then put it back together, it doesn't
bond well.

-Joe Grogan

g.balsubra manian wrote:
> Guys.,
>
> What is the bonding time for oxidised PDMS with the
> oxidised glass.
>
> Whether bonding occurs immediately after the surfaces
> get into contact.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.