stick Ni/Au on p-GaN
2006-06-15
jie bai
2006-06-15
abdou sar
2006-06-15
Jobert Van Eisden
stick Ni/Au on p-GaN
Jobert Van Eisden
2006-06-15
Jie,

Try dipping in diluted HCL 1:10 before depositing and using a wetting
layer such as 50 Angstroms of Pd or so.

Jobert van Eisden
SUNY Albany