MEMSnet Home: MEMS-Talk: Pt etchant
Pt etchant
2006-06-22
Jeehwan Kim
2006-06-22
Kirt Williams
2006-06-22
Michael D Martin
Pt etchant
Michael D Martin
2006-06-22
Use aqua regia: 3 HCl: 1 HNO3 at ~80C. You might first try this at room
temperature.

-Mike Martin
  U. of Louisville

>>> [email protected] 06/22/06 4:51 PM >>>
Dear colleagues,

I will use the Pt to protect my Si wafer surface for anodization. Is
there
any one who has a recipe for removing Pt without attacking Si surface?